斑纹铝板在染色时的影响要素引见

来路:  公布日期:2020-11-17 16:45:56  

氧化膜关于铝板的质量有很大的影响。氧化膜便是指铝板在消费的进程中的厚度、孔隙率、通明度等。铝板中膜层的厚度坚持在10um以上就可以了,孔隙率以及通明度,如许就可以失掉比拟好的染色质量。
The oxide film has great influence on the quality of aluminum plate. Oxide film refers to the thickness, porosity and transparency of aluminum sheet in the process of production. Aluminum plate in the film thickness to maintain more than 10 um on it, porosity and transparency, so you can get better dyeing quality.
染色的温度
Dyeing temperature
铝板在染色的进程中分为冷染与热染。运用冷染,所消耗的日期比拟长,在染色的进程中期颜色的平均性比拟好掌握。热染运用日期比拟短,但是在染色的进程中关于颜色的操控比拟难。热染的温度通常在10-60℃。假如在染色的进程中,温渡过高,会减小染色的吸附性,而且容易招致铝板外表发花。
The aluminum plate is dyed in cold and heat. The use of cold dyeing, the time spent is longer, in the process of dyeing the color uniformity of the middle better grasp. The use of heat dyes is relatively short, but it is difficult to control the color in the dyeing process. The temperature of heat dyeing is usually 10-60 degrees. If the temperature is too high in the process of dyeing, it will reduce the adsorption of dyeing, and easily lead to the surface of aluminium plate flower.
铝板制件质料的影响
Influence of raw materials on aluminum sheet
通常我们在消费的进程中高纯铝、铝镁、铝锰合金颠末阳极氧化当前,此中染色的功用是较好的,可以染成林林总总的颜色。关于含有硅或铜比拟重的板材,在染色的进程中只可以染成深色与玄色,比拟单调的颜色。
Usually we in the production process of high-purity aluminum, aluminum magnesium, aluminum manganese alloy after anodizing, of which the function of dyeing is the best, can be dyed into a variety of colors. For heavy plates containing silicon or copper, the dyeing process can only be dyed dark and black, relatively monotonous color.
染色液浓度


Dyeing solution concentration
铝板的浓度与染色之间存在肯定的联络,假如铝板染成浅色,此中浓度可以低落一点,染成深色浓度可以高一点。
There is a certain relationship between the concentration of aluminum plate and dyeing, if the aluminum plate dyed light, the concentration can be reduced a little, dyed dark concentration can be higher.
通常所消费的铝板资料所染比拟淡的颜色其颜色为0.1-0.39g/L,染浅色彩为1g/L,染深颜色为3-5g/L,染稀疏的颜色为10-15g/L,假如要求的染色浓度比拟高就会形成颜色不均或许会呈现浮色的景象,在干净与封闭的进程汇总容易发生流色。
Usually the lighter colors of the aluminum sheet materials are 0.1-0.39g/L, 1g/L, 3-5g/L, and 10-15g/L. If the required dyeing concentration is high, the color will be uneven or float, and flow will easily occur during the cleaning and closing process. Color.
为了增强其染色的吸附功能,如许可以运用低浓度颜色停止延伸染色,如许可以使染料可以比拟平均的浸透到氧化膜中,如许可以使染色愈加调和与结实。
In order to enhance its dyeing adsorption performance, this can use low concentration of color for extended dyeing, so that the dye can be more uniform penetration into the oxide film, this can make the dyeing more harmonious and firm.